Burst & Creep Test

Pruebas de Empaque Medico

These test methods explain the procedure for determining the ability of packages to withstand internal pressurization. The burst test increasingly pressurizes the package until the package fails. The creep test maintains a specified pressure for a specified time or until the package fails.

Prueba de fluencia

baja testing lab tijuana, packaging testing solutions ista certificate, certificado ista, ista certified laboratory, baja testing lab,

Baja Testing Lab S. de R.L. de C.V. All Rights Reserved 2020.

Contact Us for more information

+52 (664) 607-2509

INFO@bajatestinglab.com

baja testing lab tijuana, packaging testing solutions

These test methods explain the procedure for determining the ability of packages to withstand internal pressurization. The burst test increasingly pressurizes the package until the package fails. The creep test maintains a specified pressure for a specified time or until the package fails.

burst & creep test

medical packaging testing

baja testing lab tijuana, packaging testing solutions ista certificate, certificado ista, ista certified laboratory, baja testing lab,

Contact Us for more information

+52 (664) 607-2509

INFO@bajatestinglab.com